20Cr2Ni4 alloy carburized steel

20Cr2Ni4 steel is a high strength alloy carburized steel with good comprehensive mechanical properties. Its hardenability, strength and toughness are better than those of 12crni3 steel. The forging temperature is 1200 ℃, the initial forging temperature is 1150 ℃, the final forging temperature is more than 850 ℃, and slow cooling after forging. If the grains of 20Cr2Ni4 steel are coarse after forging, the coarse martensite structure will be obtained after quenching even after normalizing and subsequent carburizing.

 

GB GBT AISI
20Cr2Ni4 G20Cr2Ni4 3316

 

20Cr2Ni4 steel mechanical properties:

Tensile strength σ B (MPA): ≥ 1175
Yield strength σ s (MPA): ≥ 850
Reduction of area ψ (%): ≥ 45
Impact toughness value α kV (J / cm2): ≥ 78 (8)